    Composition:
     
    [1] by the polyurethane resin and modified epoxy resin, asphalt, anti-rust paint and additives such as grinding fine filter made of two-component coating.
     
    Performance:
     
    Good film toughness, strong adhesion, wear resistance, corrosion resistance and excellent corrosion resistance.
     
    Be applicable:
     
    Applicable to underground pipes, including buried in a variety of soil conditions and underground structures and flooding structures, steel piers and other terminals.
     
    Specifications:

    project

    index

     

    Appearance of paint film

    Smooth and smooth

     

    Drying time h
     
    (25 ± 1 ℃)

    Table dry ≤

    6

    Hard work ≤

    24

     

    Flexibility mm ≤

    5

     

    Adhesion (circle method) level ≤

    3

     

    Impact resistance kg · cm

    40

     

    Non - volatile content% ≥

    70

     

    Construction Parameters:
     
    Proportion: see the barrel paste
     
    Applicable period: 8 hours
     
    Thinner and dosage: special thinner, ≤ 5%
     
    Painting method: brush, roller or spray
     
    Painting interval: the shortest 4 hours, up to 3 days.
     
    Film thickness: wet film: 200μm dry film: 120μm
     
    Theoretical dosage: 250g / m
     
    Surface treatment: Remove the surface of the oil stains, dust, welding slag, oxidized into loose rust, keep the surface dry and pollution-free.
     
    Supporting primer: IPN8710 anti-corrosion primer, IPN8710-4 thick slurry-type anti-corrosion primer.
     
    Storage period: 12 months
     
    Precautions:
     
    1. Products should be stored in a cool, ventilated and dry place, isolated fire, away from heat.
     
    2. This product is thick slurry coating can be thick coating construction is not appropriate to hang, open the barrel after the general can not brushing with thinner.
     
    3. Paint durations are too long, will be slightly precipitated, should be stirred before use.
     
    4. After preparation of paint, curing in summer for 20 minutes, 1.5-2 hours after curing in winter construction, generally used within 8 hours, otherwise the viscosity thickening, difficult to construction.
     
    5. Primer surface can be painted after the paint, room temperature interval should not be more than two days, otherwise it will affect the combination of layers, coating the time between the topcoat also to dry the surface as well.
     

    上一篇:没有了
    下一篇:IPN8710 corrosion-resistant steel pipe
    Three cloth four oil
    Cement mortar anti -
    Double - sided submer
    Prefabricated polyure
    API Spiral steel pipe
    l290 Spiral steel pip
    q345b Spiral steel pi
    L360 spiral steel pip